Ku languteka: phoyizeni yo tshwuka yo vonikela
Znic oxide Nhlayo:min 50%
Active Znic oxide Nhlayo:min.93%
Ndhawu yo karhi ya le henhla:25m2/g
density:3.4g/cm3
Ku languteka: phoyizeni yo tshwuka yo vonikela
Znic oxide Nhlayo:min 54%
Active Znic oxide Nhlayo:min.93%
Ndhawu yo karhi ya le henhla:20-30m2/g
density:3.6g/cm3
Muxaka: Binary ethylene propylene rubber
Ku languteka na xiyimo: xo basa (xi vonaka kumbe lexi vonakaka kahle) xa blocky
Nhlayo ya ethylene: 59%
Nhlayo ya propylene: 41%
Mooney viscosity: ML(1+4)125°C 79
Vukulu: 25kg/bag
MOQ: 25kg
Ku paka: ebokisini
Ku languteka na xiyimo: xo basa (xi vonaka kumbe lexi vonakaka kahle) xa blocky
Nhlayo ya ethylene: 72%
Nhlayo ya propylene: 28%
Ku tsindziyela ka Mooney: ML(1+4)100°C 30
Vukulu: 25kg/nkwama
MOQ: 25kg
Ku paka: ebokisini
Ku languteka na xiyimo: xo basa (xi vonaka kumbe lexi vonakaka kahle) xa blocky
Nhlayo ya ethylene: 72%
Nhlayo ya propylene: 28%
Ku tsindziyela ka Mooney: ML (1+4) 100°C 44
Vukulu: 25kg/nkwama
MOQ: 25kg
Ku paka: ebokisini