Ku languteka na xiyimo: xo basa (xi vonaka kumbe lexi vonakaka kahle) xa blocky
Nhlayo ya ethylene: 72%
Nhlayo ya propylene: 28%
Ku tsindziyela ka Mooney: ML(1+4)100°C 30
Vukulu: 25kg/nkwama
MOQ: 25kg
Ku paka: ebokisini
Ku languteka na xiyimo: xo basa (xi vonaka kumbe lexi vonakaka kahle) xa blocky
Nhlayo ya ethylene: 72%
Nhlayo ya propylene: 28%
Ku tsindziyela ka Mooney: ML (1+4) 100°C 44
Vukulu: 25kg/nkwama
MOQ: 25kg
Ku paka: ebokisini
Ku languteka na xiyimo: xo basa (xi vonaka kumbe lexi vonakaka kahle) xa blocky
Nhlayo ya ethylene: 72%
Nhlayo ya propylene: 38%
Ku tsindziyela ka Mooney: ML (1+4) 125°C 60
Vukulu: 25kg/nkwama
MOQ: 25kg Ku paka
: ku vekiwa emabokisini
Muxaka: Binary ethylene propylene rubber
Ku languteka na xiyimo: xo basa (xi vonaka kumbe xi vonaka kahle) xa blocky
Nhlayo ya ethylene: 59%
Nhlayo ya propylene: 41%
Mooney viscosity: ML (1+4) 100°C 44
Vukulu: 25kg/nkwama
MOQ: 25kg
Ku paka: ebokisini
Muxaka: Binary ethylene propylene rubber
Ku languteka na xiyimo: yo basa (yo vonaka kumbe yi vonaka kahle) blocky
Nhlayo ya ethylene: 52%
Nhlayo ya propylene: 48%
Mooney viscosity: ML (1+4) 100°C 80
Vukulu: 25kg/nkwama
MOQ: 25kg
Ku paka: ebokisini