Qaybta Alaabta

Rubbers-synthetic: Guryaha faahfaahsan, Faa'iidooyinka, iyo Codsiyada

1. Fluororubber (FKM)

  • Guryaha:

    • Iska caabin heerkul aad u daran (-20°C ilaa +250°C).

    • Iska caabin aan caadi ahayn ee saliidaha, shidaalka, dareerayaasha, asiidhka, iyo saldhigyada.

    • Xoog cufan oo sarreeya, dejin cadaadis hooseeya, iyo xasilooni kiimikaad oo aad u wanaagsan.

    • Ololka u adkaysta iyo ozone u adkaysta.

  • Faa'iidooyinka:

    • Waxay u adkaysataa kiimikooyinka gardarada leh iyo bay'ada cadaadiska sare leh.

    • Nolosha adeeg dheer ee hawada hawada iyo codsiyada baabuurta.

  • Codsiyada:

    • Xirmooyinka shidaalka ee diyaaradda, O-rings, iyo gaasaska.

    • Xirmooyinka gudbinta baabuurta, tuubooyinka injiinka, iyo qaybaha turbocharger.

    • Dahaarka qalabka wax lagu farsameeyo iyo gaasaska.

2. Rubber Chloroprene (CR)

  • Guryaha:

    • Iska caabin saliid dhexdhexaad ah (ka fiican caagga dabiiciga ah laakiin ka yar FKM).

    • Dab-demiska oo leh sifooyin is-daminta.

    • Iska caabbinta cimilada wanaagsan (UV, ozone, iyo qoyaan).

    • Dabacsan heerkulka hoose (-40°C ilaa +120°C).

  • Faa'iidooyinka:

    • Kharash-ku-ool ah oo leh habayn sahlan (extrusion/samaynta).

    • Xoogga farsamada sare iyo caabbinta naaxinta.

  • Codsiyada:

    • Suudhadhka qoyan, galoofyada, iyo tuubooyinka warshadaha.

    • Xabagta kabaha iyo dhismaha.

    • Jaakadaha fiilada iyo xuubka saqafka.

3. Rubber Nitrile Hydrogenated (HNBR)

  • Guryaha:

    • Iska caabbinta kulaylka oo la xoojiyey (ilaa +150°C) marka loo eego NBR.

    • Iska caabbinta sare ee saliidaha, dareerayaasha hawo-biyoodka, iyo aminyada.

    • Xoog adkaysi sare iyo iska caabin daal.

    • U adkaysiga hoose ee gaasaska.

  • Faa'iidooyinka:

    • Waxay xajistaa dabacsanaanta iyadoo ay sii dheeraato soo-gaadhista kiimikooyinka adag.

    • Cimri ka dheer NBR xaaladaha ba'an.

  • Codsiyada:

    • Qalabka qodista saliidda iyo gaasta ( baakadaha, shaabadadaha).

    • Suunka wakhtiga baabuurta, qaybaha la isku duro ee shidaalka, iyo shaabadihii turbocharger.

    • Dhululubada haydarooliga warshadaha.

4. Caag Silikoon ah (VMQ)

  • Guryaha:

    • Heerkulka aadka u ballaadhan (-60°C ilaa +200°C).

    • Balaasti sare (ilaa 1000% elongation).

    • Dabool koronto oo heer sare ah iyo xasilloonida kulaylka.

    • noole la jaanqaadi kara oo aan toos ahayn.

  • Faa'iidooyinka:

    • Waxay ilaalisaa dabacsanaanta deegaanka cryogenic iyo heerkul sare.

    • Iska caabbinta UV, ozone, iyo cimilada.

  • Codsiyada:

    • Qalabka caafimaadka (kateetarka, maqaar-galaha).

    • Qaybaha elegtarooniga ah (insulators, keypads).

    • Gaasaska heerkulka sare ee foornooyinka iyo matoorada.

5. Rubber Fluorosilicone (FVMQ)

  • Guryaha:

    • Waxay isku daraysaa iska caabbinta kiimikada FKM iyo dabacsanaanta VMQ.

    • Heerkulka: -50°C ilaa +230°C.

    • U adkaysta shidaalka, saliidaha, iyo dareerayaasha hawo-biyoodka.

    • Dejinta cadaadiska hooseeya iyo adkeysiga wanaagsan.

  • Faa'iidooyinka:

    • Wuxuu ku shaqeeyaa heerkul sare iyo heerkul hoose labadaba.

    • U adkaysta bararka shidaalka duulista.

  • Codsiyada:

    • Qaybaha nidaamka shidaalka ee diyaaradda (valves, seals).

    • Baakadaha iyo isku xidhayaasha badda hoostooda hoos mara.

    • Dareemayaasha baabuurta iyo nidaamyada xakamaynta qiiqa.

6. Ethylene Propylene Diene Monomer (EPDM)

  • Guryaha:

    • Osoone heersare ah iyo iska caabbinta cimilada.

    • Awood sare oo koronto ah iyo iska caabbinta biyaha.

    • Heerkulka: -50°C ilaa +150°C.

    • Dareemidda gaaska hooseeya.

  • Faa'iidooyinka:

    • Inta badan kharash-ku-ool ah codsiyada dibadda.

    • Gariir heersare ah oo qoyan iyo dhimista qaylada.

  • Codsiyada:

    • Gawaarida cimilada, tuubooyinka hiitarka, iyo xidhmooyinka muraayadaha hore.

    • Xuubabka saqafka iyo balliyada.

    • Xakamaynta fiilooyinka korantada iyo suumanka gudbinta korontada.


XIDHIIDHYADA DEGDEGGA AH

Alaabooyinkayaga

MACLUUMAADKA XIRIIRKA

Kudar: No.33, Lane 159, Wadada Taiye, Degmada Fengxian, Shanghai
Tel / WhatsApp / Skype: +86 15221953351
Xuquuqda daabacaadda     2023 Shanghai Herchy Rubber Co., Ltd. Khariidadda goobta |   Siyaasadda Qarsoonnimada | Taageerada By Leadong.