Kabaha Iska caabbinta kulaylka Xoog Sareeye Ethylene Propylene Rubber-EPR

Muuqashada iyo xaaladda: caddaan (daah-furan ama hufan) xannibaad
Nooca monomer-ka saddexaad iyo waxa ku jira: ENB, 2.0%
Ethylene content: 62%
Mooney viscosity: ML(1+4)125°C 53
Cabbir: 25kg/block
MOQ: 25kg
Xidhmada: Sanduuqa
  • J-2080

Helitaanka:
Tirada

Kabaha Ethylene Propylene Rubber ee Waxqabadka Sare - EPR Raw Raw

Sharaxaada Alaabta

Soo bandhigida Kabaha waxqabadka Sare ee Ethylene Rubber Propylene - EPR Raw Rubber. Xaruntan caagga ah ee horumarsan waxaa loogu talagalay in lagu bixiyo waxqabadka aan la barbar dhigi karin ee kabaha, hubinta raaxada ugu badan, adkeysiga, iyo isku halaynta.

Astaamaha Muhiimka ah

  1. Xoog Sare : Rabadhkayaga EPR ee ceyriinka ah wuxuu ku faanaa xoog adkaysi aan caadi ahayn, isagoo siinaya taageero iyo xasillooni aan la qiyaasi karin dhammaan naqshadaha kabaha.

  2. Iska caabinta kulaylka : caagkani wuxuu u taagan yahay heerkul sare, ilaalinaya qaabkiisa iyo waxqabadkiisa xitaa xaaladaha ugu daran.

  3. Nuugista Shoogga Gaarka ah : Caaggu waxa loo qaabeeyey sifooyin shoog-nuugaya oo aad u wanaagsan, oo cagta ka ilaalinaya saamaynta iyo shoogga.

  4. Xiro iska caabin : caaggu aad buu ugu adkaysanayaa xoqidda iyo xidhashada, isaga oo hubinaya in kabahaagu ay ilaalin doonaan muuqaalkooda iyo waxqabadkooda waqti ka dib.

  5. Si fudud loo habeeyo : Xarunta caagga ah waxaa loogu talagalay fududaynta wax-is-beddelka iyo qaabeynta inta lagu jiro habka wax-soo-saarka.

Codsiga

Kabaha Ethylene Propylene Rubber ee Waxqabadka Sare - EPR Raw Rubber waxaa si gaar ah loogu qaabeeyey in loo isticmaalo soo saarista kabaha. Isticmaalka caagga ceyriinka ah ee EPR, soo saarayaasha kabaha waxay abuuri karaan kabo raaxo leh, waara, oo la isku halayn karo oo u taagan isticmaalka soo noqnoqda iyo xaalado daran.

Gabagabo

Kabaha Ethylene Propylene Rubber ee Waxqabadka Sare - EPR Raw Rubber waa doorashada ugu fiican ee soo saarayaasha kabaha ee raadinaya xarun caag horumarsan oo isku dareysa xoog sare, caabbinta kulaylka, nuugista naxdinta, xidhashada caabbinta, iyo fududaynta habaynta. Iyada oo waxqabadkeeda la isku halleyn karo iyo adkeysiga, xaruntan caaggu waxay hubisaa raaxada, cimri dhererka, iyo ku-tiirsanaanta noocyo badan oo kabo ah.


Kii hore: 
Xiga: 

XIDHIIDHYADA DEGDEGGA AH

Alaabooyinkayaga

MACLUUMAADKA XIRIIRKA

Kudar: No.33, Lane 159, Wadada Taiye, Degmada Fengxian, Shanghai
Tel / WhatsApp / Skype: +86 15221953351
Xuquuqda daabacaadda     2023 Shanghai Herchy Rubber Co., Ltd. Khariidadda goobta |   Siyaasadda Qarsoonnimada | Taageerada By Leadong.