Di we aw i tan ɛn di kɔndishɔn: wayt (transparent ɔ translucent) blɔk
Itilɛn kɔntinyu: 55%
Prɔpilin kɔntinyu: 45%
Mooney viskɔsiti: ML(1+4)100°C 33
Sayz: 25kg/bag
MOQ: 25kg
Pak: bɔks
Di we aw i tan ɛn di kɔndishɔn: Bij ɔ pale yɔlɔ blɔk
Tɔd monoma tayp ɛn kɔntinyu: ENB, 3.4%
Ɛtilin kɔntinyu: 64.6%
Mooney viskɔsiti: ML(1+4)125°C 32
Ɔyl kɔntinyu: 100%
Sayz: 25kg/blɔk
MOQ: 25kg
Pak: bɔks
Di we aw i tan ɛn di kɔndishɔn: Bij ɔ pale yɔlɔ blɔk
Tɔd monoma tayp ɛn kɔntinyu: ENB, 4.5%
Ɛtilin kɔntinyu: 55.5%
Mooney viskɔsiti: ML(1+4)125°C 55
Sayz: 25kg/blɔk
MOQ: 25kg
Pak: bɔks
Di we aw i tan ɛn di kɔndishɔn: Beij ɔ pale yɔlɔ blɔk
Tɔd monoma tayp ɛn kɔntinyu: ENB, 4.5%
Ɛtilin kɔntinyu: 59.5%
Mooney viskɔsiti: ML(1+4)125°C 47
Ɔyl kɔntinyu:10%
Sayz: 25kg/blɔk
MOQ: 25kg
Pak: bɔks