Sigilan minnu ka dɔgɔn : Etilɛni poropilɛni diyɛni monomɛri (EPDM) lastikuw labɛncogo laban
Dajirali:
An bɛ an ka sigilan kura jira minnu ka dɔgɔn, minnu dilannen don ni Etilɛni Propilɛni Diyɛni Monɔmɛri (EPDM) lastikuw ye, minnu dilannen don walasa ka izini suguya caman ka ɲinini gɛlɛnw dafa. An ka sigilanw bɛ baarakɛcogo kɛrɛnkɛrɛnnen ni dannaya di, o b’a to u ye sugandili sanfɛla ye sigilanw tali la.
.
O kɛcogo in bɛ fanga sɔrɔcogo ɲuman sabati ani ka musaka dɔgɔya izini baara suguya caman na.
2. Furakɛcogo min musaka ka dɔgɔ:
An ka sigilanw dilannen don ni tigitigi ye ani u bɛ baara kɛ ni fɛɛrɛ kɔrɔw ye, u bɛ nafa caman di wariko la min ɲɔgɔn tɛ. U musaka dɔgɔyali b’u kɛ sugandi ye min bɛ mɔgɔ ɲɛnajɛ jagokɛlaw bolo minnu b’a fɛ ka musakaw dɔgɔya k’a sɔrɔ u bɛ sariyakolo ɲumanw mara.
3. Funteni kunbɛnni ka bon :
EPDM lastikuw faralen ɲɔgɔn kan min bɛ kɛ an ka sigilanw na, o bɛ funteni kunbɛncogo kabakoma jira, o b’a to u bɛ se ka funteni jugumanba muɲu k’a sɔrɔ u ma u datugucogo tiɲɛ walima ka bɔnɛ u la. O fɛɛrɛ in bɛ baarakɛcogo basigilen sabati hali sigida gɛlɛnw na.
4. Minimal Compression Set and Permanent Deformation:
An ka sigilan minnu ka dɔgɔn, olu dabɔra walasa k’u cogoya n’u dafalen mara degun kɔrɔ, ka a to compression set fitinin ani deformation permanent. Nin yɔrɔ in bɛ baarakɛcogo kuntaalajan ni sigicogo seko dannamɔgɔ garanti.
.
Ka fara o kan, u ka masin fanga ka bon, o bɛ a to u ka mɛn ani u ka mɛn hali doni girinmanw ni degunw kɔrɔ.
Kuncɛli :
An ka sigilan minnu ka dɔgɔn, n’olu dilannen don ni Ethylene Propylene Diene Monomer (EPDM) lastikuw ye, olu bɛ fura bɛɛ di sigicogo baarakɛcogo ma izini suguya caman kɔnɔ. Ni u ka density ka dɔgɔn, u musaka ka dɔgɔ, u ka funteni ka bon, u ka compression set ka dɔgɔn, ani u ka kemikaliya kɛlɛli ka ɲi, o sigilanw bɛ baara kɛ min bɛ se ka da a kan ani min bɛ baara kɛ ka ɲɛ. An ka sigilanw sugandi minnu ka dɔgɔn walasa ka sigicogo ɲuman sɔrɔ min bɛ aw mago kɛrɛnkɛrɛnnenw ɲɛ ani min bɛ tɛmɛ aw jigi kan.