Etileni hakɛ: 72%
Propylene hakɛ: 28%
Mooney viscosity: ML (1+4) 100°C 44
Bonya: 25kg/bag
MOQ: 25kg
Packing: boxed
A cogoya ni a cogoya: finman (a jɛlen don walima a bɛ yeelen bɔ) bloki
Etilɛni hakɛ: 72%
Propylene hakɛ: 38%
Mooney viscosity: ML (1+4) 125°C 60
Bonya: 25kg/bag
MOQ: 25kg
Packing: boxed