Views: 0 Author: Site Editor Bɔli waati: 2023-08-13 Bɔyɔrɔ: Yɔrɔ
Jogo ni baarakɛcogo
Kuloropɛrɛni lastikuw (CR) ye kuloropɛrɛni lastikuw nɔrɔlen fɛnba ye, nɔrɔlan bɛ se ka kɛnɛya nɛnɛ na so funteni na, nɔrɔli fanga fɔlɔ ka bon kosɛbɛ, fanga sigili teliya la, sirili fanga ka bon, baara bɛɛ lajɛlen ɲumanba, baara kɛcogo caman na, a bɛ se ka lastikuw siri, fari, finiw, fari, plastiki, jiri, papiye, gilasi, seramiki, bɛton, nɛgɛ ani fɛn caman wɛrɛw, o la kuloropɛri lastikuw nɔrɔlen fana bɛ wele O la, neopɛrɛni lastikuw nɔrɔlan fana tɔgɔ ye ko 'universel nɔrɔ Neoprene rubber adhesive bɛ sɔrɔ solvent-based, emulsion type ani solvent-free liquid type, solvent-based bɛ tila ka kɛ mixte ni graft suguya ye. O ɲagaminenw ye CR nɔrɔlan saniyalenw ni CR nɔrɔlenw ye minnu kɔnɔ fasaw bɛ sɔrɔ, ani CR nɔrɔlenw minnu sɛgɛsɛgɛra ni resin ye. Graft suguya ye neoprene rubber ni methyl méthacrylate ani monomère solution wɛrɛw graft copolymerization of the adhesive ye. Sisan, neopɛrɛni lastikuw nɔrɔlan min bɛ kɛ ni furaji ye, o de bɛ kɛ ka caya hali bi, fɛɛrɛw ka kan ka tigɛ walasa ka dɔ bɔ nɔgɔ baga la, ka kɛɲɛ ni sigida magow ye.
Fɔlɔ, neopɛrɛni lastikuw nɔrɔlan suguya ɲagaminen
Neoprene lastikuw ɲagaminen kɔrɔ ye ko neoprene lastikuw ɲagaminen (walima a ma ɲagami) a wulilen don furajiw ɲagaminen na, ka resinw, farikolo tangalanw, fasaw ani faralifɛn wɛrɛw fara a kan.
Kɔrɔyafɛn, fasa ani faralifɛn wɛrɛw ka kɛ fɛn kelen walima fɛn fila ye min bɛ kɛ ni furaji ye.
1、 Karamɔgɔya
(1), a daminɛ fanga nɔrɔlen, neoprene lastikuw ka nɔgɔn ka kristalize, nɔrɔlen coating ani ja stacking, a bɛ se ka kɛ instantaneous crystallization plus ni
Tackifier resin, min bɛ fanga nɔrɔlenba jira fɔlɔ. . (3), sirili fanga ka bon, neoprene lastikuw ka kristalini ka bon, jɛɲɔgɔnya fanga, ani o cogo la CR nɔrɔli fanga ka bon. (4), kunnafonidilanw kɛlɛli ɲuman, tulu kɛlɛli, ji kunbɛncogo ɲuman, kemikaliya kunbɛncogo ɲuman. (5) Nɔrɔlan bɛ nɔgɔya, a bɛ wuli ani a tɛ se ka sɔgɔsɔgɔ ani ka yɛrɛyɛrɛ. (6), a bɛ mɛn ka ɲɛ, a bɛ yeelen bɔ kosɛbɛ, a bɛ se ka ozɔni kɛlɛ, a bɛ se ka kɔrɔya fiɲɛ na, a tɛ tasuma bali. Lastikuw ni nɛgɛ sirili so kɔnɔ san 20 sirili fanga bɛ ɲini ka dɔgɔya. (7), baarakɛcogo caman, nɛgɛ ni nɛgɛ tɛ fɛn minnu na, olu nɔrɔli ka ɲi, kɛrɛnkɛrɛnnenya la fɛn suguya minnu sirilen don ɲɔgɔn na, nɛgɛdaga wɛrɛw minnu dilannen don ni lastikuw ye, olu tɛ se ka suma ɲɔgɔn ma. (8), a baara ka nɔgɔn, kola jalen kɔfɛ, ni a magara siɲɛ kelen, a sirili teliya la k’a sɔrɔ a ma degun ka mɛn, o bɛ se ka kɛnɛya kɛnɛma funteni na. (9), funteni kunbɛncogo man ɲi, nɛnɛ kunbɛncogo man ɲi. (10), neopɛrɛni nɛgɛ min bɛ kɛ ni furaji ye, o fanba bɛ ni baga ni nɔgɔ hakɛ dɔ ye.
Neoprene nɛgɛ ɲagaminen ye nɛgɛ ye min bɛ se ka kɛ kosɛbɛ, a bɛ kɛ ka caya izini dilanni na ani don o don ɲɛnamaya kɔnɔ. Kɛrɛnkɛrɛnnenya la A bɛ Kɛ kosɛbɛ iziniw dilanni na ani don o don ɲɛnamaya la, kɛrɛnkɛrɛnnenya la sanbara dilanni, minɛnw, jɔli, mobili ani izini wɛrɛw la ni hakɛ caman ye.
2.Daɲɛw labɛncogo
Neoprene lastikuw ɲagaminen bɛ kɛ ni neoprene lastikuw ye, tackifying resin, nɛgɛ oksizɛni, furajiw, farikolo tangalanw, fasalanw, teliyalanw,
Crosslinking agent ani a ɲɔgɔnnaw.
I. Kuloropɛrɛni ka lastikuw
Kuloropɛrɛni lastikuw, n’a bɛ fɔ fana ko polikuloropɛrɛni, o ye 2-kuloro-1,3 butadiyɛni ye i n’a fɔ fɛn fɔlɔ min bɛ kɛ ni emulsiɔn polimerizasiyɔn ye ani a ye ɛlastomɛri sugu dɔ dilan.
Elastomɛri (Elastomɛri) ye. Kuloropɛrɛni lastikuw ye fɛn finman walima jɛman ye walima fɛn gɛlɛn gɛlɛn, a bɛ se ka wuli ka bɔ a nɔ na, a bɛ nɔrɔ ka ɲɛ, a bɛ se ka sɔgɔsɔgɔ kosɛbɛ ani a bɛ janya. Kɔrɔya, funteni, tulu ani kemikaliya kunbɛncogo ɲuman. Weelecogo ni ozɔni kɔrɔya kɛlɛli ye filanan ye etilɛni poropilini lastikuw ni butili lastikuw kɔfɛ. Funteni kunbɛnni ani nitirili lastikuw. Asidi inorganique ni alkali sɔgɔli kunbɛncogo ɲuman. Tasuma-fagalan hakɛ dɔ bɛ a la. Funteni kunbɛnni ka jugu dɔɔni, kuran sɔgɔli man ɲi.
2, tackifying resin ye
Tackifier resin ye solvent-based neoprene adhesive yɔrɔ nafama dɔ ye, min bɛ se ka cohesive fanga, nɔrɔcogo, funteni kunbɛnni, ji kunbɛncogo ani kɔrɔya kunbɛncogo ɲɛ.
Cɛnimusoko ni kɔrɔya kɛlɛli. Tackifier resin minnu bɛ kɛ, olu ye thermo-reactive alkyl phenolic resins, petoroli resin, terpene phenolic resin, terpene resin, rosin-modified phenolic resin, gumarone resin, rosin esters, poly a-methylstyrene ani a ɲɔgɔnnaw. Olu la, tert-butylphenol formaldehyde resin (2402 resin) de bɛ nɔ ɲuman bila. Tackifier resin bɛ se ka nɔ foyi bila neoprene rubber ka kristali la. Terpene phenolic resin ye resin thermoplastique non réactive ye min bɛ se ka nɔrɔlen mara waati janya, ka nɔrɔlan kɛ nɔgɔ ye, Gumarone resin fana bɛna neoprene nɔrɔlen kɛ
Gumarone resinw fana bɛ dɔ fara dɔɔni di neoprene nɔrɔlenw sirili fanga kan. Kuloropɛrɛni lastikuw AF ye asidi karɔbɔliki CR ye, n’o ye nɔrɔlen sirili fanga min dilannen don, o bɛ sigi senkan teliya la funteni kunbɛnni na, delaminasiyɔn kɛlɛli ka bon, nka, k’a sababu kɛ a ka walekɛcogo ye, nɔrɔlan ka sɔgɔsɔgɔninjɛ bɛna wuli a maracogo la, o bɛ bɔ oksizɛni manje ka ɲɔgɔndan nɔ na. O la, AF neoprene nɔrɔli labɛnni na walasa ka sɔgɔsɔgɔninjɛ sabatili ɲuman sɔrɔ ani ka baarakɛcogo bɛɛ lajɛlen sɔrɔ, a ka kan ka fara a kan ka kɛ resin 2402 hakɛ bɛrɛbɛrɛ ye, wa okisidi manje ka kan ka kɔn ka kɛ ni resin ye walasa ka kelatiw sɔrɔ, o bɛ se ka ɔkisizɛni manje ni hidrɔkisili tilennenw bali ani ka dɔ fara a sɔgɔli sabatili ni funteni kunbɛnni kan sigida la.
3, nɛgɛ oksizɛni
Nɛgɛ ɔkisizɛni minnu bɛ neopɛrɛni nɛgɛmafɛnw na, olu jɔyɔrɔ naani bɛ u la: asidi minɛbaga, sɔgɔsɔgɔninjɛ fura, vulkanizelan, resin kɛbaga. Waati tɛmɛnen kɔfɛ, neopɛrɛni lastikuw bɛna kuloridi idɔrɔzi hakɛ fitininw bɔ, a bɛ se ka polimɛriw tiɲɛ ka taa a fɛ, wa a bɛna nɛgɛw ni fiɲɛw tiɲɛ, ka nɛgɛ oksizɛni fara a kan, o bɛ se ka kuloridi idɔrɔzi minɛ walasa tiɲɛni kana taa ɲɛ. Nɛgɛ oksizɛni minnu bɛ kɛ ka caya, olu fanba ye zinki ɔkisidi ni manje ɔkisidi ye. Okisidi magnɛsiyɔmu ka baara ye ka asidi minɛ, ka kɔn ka a kɛ, ka sɔgɔsɔgɔninjɛ kɛlɛ, ka vulkanize, a ɲɔgɔnnaw A ye neoprene nɛgɛmafɛn ye min nafa ka bon kosɛbɛ. Manzeyɔmu ɔkisidi ni resin ka kɔn ka ɲɔgɔn sɔrɔ, o bɛ se ka nɔrɔlenw ka funteni kunbɛncogo ɲɛ ani ka delamination precipitation bali, magnesium oxide hakɛ bɛ nɔ bila pre-reaction nɔ na ani nɔrɔli jogo bɛ nɔ bila, ni magnesium oxide hakɛ bɛ bonya, funteni caman fanga bɛ bonya, nka nɔrɔji sabatili bɛ dɔgɔya. Okisidi manje farali bɛ se ka filimu nɔrɔlen teliya kosɛbɛ walasa a ka ja, wa a bɛ se ka sirili fanga fɔlɔ ɲɛ kosɛbɛ, o bɛ se ka kɛ sababu ye ka bɔ ɔkisizɛni manje yeelenma tobilen na walima ɔkisizɛni manje min bɛ baara la. Ɔkisizɛni manje jɛman ye mugu finman ye min tɛ fɛn wɛrɛ ye, kasa tɛ a la, wa a tɛ diya. Danyɔrɔ 3. 58, wuliyɔrɔ 28520C, tobiliyɔrɔ 36000C fiɲɛ na, o bɛ se ka gazi ɲuman ni ji minɛ dɔɔni dɔɔni walasa ka karɔbɔni manje basigilen bɔ . Zɛnki ɔkisidi min farala kuloropɛrɛni nɔrɔlen kan, o bɛ se ka jɔyɔrɔ ta asidi minɛni na, nka o ye vulkanizelan ye, o tɛ laɲini ye bawo kuloropɛrɛni nɔrɔlen fanba bɛ kɛnɛma funteni kɛ ni nɛnɛ ye ka da a kan kemikoro tɛna vulkanizasiyɔn lase, nka o fana bɛ kɛ sanji jukɔrɔla marali la. O waati kelen na, zinki ɔkisizɛni bɛ se ka nɔrɔji kɛ fɛn nɔgɔlen ye, walasa nɔrɔlen filimu ka nɔrɔ, a bɛ i n’a fɔ a jalen don a tɛ ja, a bɛ kɛ ka poliyuritan fomu siri, zinki ɔkisizɛni bɛna kɛ sababu ye ka fɛn in kɔrɔya. Ka da kun minnu fɔra sanfɛ, olu bɛ se ka zinki ɔkisidi tiɲɛ tiɲɛ na, jamana wɛrɛw ka kuran minɛn minnu bɛ ni CR nɔrɔlen ye, olu ma zinki ɔkisidi fara a kan, kola bɛ kɛnɛya ani a tɛ layɛrɛ. Ni zinki ɔkisidi tɛ, o fana bɛ se ka siri fanga wajibiyalen sɔrɔ, nka a bɛ se ka kɛ fana ka nɔrɔlen saniyalen jeni, walasa ka nɔrɔlan bali ka mara waati jan kɔnɔ
Aw bɛ jeli ni sanji bɔ, wa a tɛna kɛ sababu ye ka kola fasa faranfasi. Ni neoprene nɔrɔlen sirili bɛ kɛ ni funteni caman ye, aw bɛ zinki ɔkisidi ultra-fine active (zinki ɔkisidi active ultra-fine) hakɛ dɔɔni (1~3 copies) fara a kan, o nafa ka bon.
4, farikolo tangalan
Walasa ka lastikuw toli bali, ka kɔrɔya kunbɛncogo ɲɛ, ka baara kɛ waati janya, walasa ka yɔrɔw sirilenw muɲuli sabati, a ka kan ka farikolo tangalan bɛnnen fara a kan. Oksidan D min bɛ kɛ ka ɲɛ, o ka ɲi kosɛbɛ nka a bɛ nɔgɔ ani ka kansɛri bila mɔgɔ la, o ka kan ka bila ODA, RD, 264, a ɲɔgɔnnaw na o nɔ na. Antioxydant 2246 fana bɛ se ka kɛ, nka a bɛna kɛ sababu ye ka kulɛri caman wuli, kulori bɛ sɔrɔ furajiw la, a bɛ kɛ bulu jɛman ye, bulu ka kɛ wuluwulu yeli ye latex la, o ye pinki ye.
5, furaji
Solvent ye solvent-based neoprene adhesive indispensable caman ye a yɔrɔw la, adhesive baarakɛcogo bɛ nɔba bila. Kuloropɛrɛni lastikuw wulicogo hakɛ ye 9,2 ~ 9,4 ye, a bɛ wuli dɔɔni bɛnzɛni, toluyɛni, dikuloromɛtan, kuloridi mɛtilɛni, kuloridi mɛtilɛni, trikuloromɛtan, 1, 1, 1-tirikuloroɛtan, karɔbɔni tetarasikilini, trikuloroetilɛni, butanoni, a ɲɔgɔnnaw na, a bɛ wuli dɔɔni sikɔlɔhɛksan, etili la asetati, metil asetati, isoporopili asetati, asetɔni, minnu tɛ se ka wuli n-alkan, n-hɛptan, n-hɛptan, gazi solvant, isoporopanɔli ani a ɲɔgɔnnaw na. Furakɛcogo minnu man ɲi ani fura minnu tɛ furaji ye, olu dɔrɔn tɛ neoprene lastikuw wulilen ye, nka ni u ɲagaminen hakɛ bɛnnen don, u bɛ se ka neoprene lastikuw fana wuli. Neoprene lastikuw ka fɛnɲɛnamafagalanw wulicogo, a nɔrɔli sɔgɔli, a sɔgɔli sabatili, nɔrɔli jisigicogo, a sɔgɔli mara waati, a nɔrɔli fanga fɔlɔ, a jalen teliya, a sirili fanga, a marali sabatili, a ka funteni dɔgɔyali, a tasuma, a bɔgɔbɔli, a baga, a nɔgɔli, a nɔrɔli musaka, a ɲɔgɔnnaw bɛ nɔba bila a la.
6, fasa
Filler in the solvent-based neoprene adhesive tɛ baara kɛ kosɛbɛ, barisa adhesive solvent hakɛ, a solide hakɛ ka dɔgɔn, a bɔli ka nɔgɔn, a tɛ se ka jɔyɔrɔ makɔnɔnen ta. Ni karɔbɔni kalisiyɔmu activé superfine kɛra, a bɛ se ka sabati ka tɛmɛ. Ani tali mugu ultrafine, silica ultrafine, silikati aluminiyɔmu ultrafine, bɔgɔ ultrafine baara bɛ se ka mara waati kunkurunnin dɔrɔn kɔnɔ ka sabati. Wa a laban na, sanji bɛna Nà.
7, crosslinking (kɛrɛnkɛrɛnnenya la).
Crosslinking agent, n’a bɛ fɔ fana ko curing agent, o bɛ se ka neoprene rubber adhesive furakɛli teliya teliya, ka jɛɲɔgɔnya fanga ɲɛ, ka funteni kunbɛn, ka ji kɛlɛ, ka tulu kɛlɛ, ka kemikɛli kɛlɛ, ka kɔrɔya kunbɛn. A ka ca a la, a bɛ kɛ ka poliisosiyanati sɔgɔsɔgɔninjɛ furakɛ, i n’a fɔ tetaraisosiyanati. Poliisosiyanati crosslinking agent ni reactivité caman, fara chloroprene adhesive kan 2~3h bɛ se ka crosslinked gel, i n’a fɔ fila-component adhesive, sani a ka baara kɛ ni a bilali ye, ka a ɲagami ani ka a kɛ o yɔrɔnin bɛɛ.
8, teliyalan
Promoteur ye ka vulcanization sabati walasa ka funteni kunbɛncogo ɲɛ ani ka fɛnw fara a kan, i n’a fɔ vinylthiourea (NA-22), diethylthiourea (DE-TU), diphenylthiourea (promoteur C), diaminodiphenylméthane, hakɛ caman ye 0,25 ~ 1 share ye. Mɔgɔ dɔw bɛ sɔrɔ kuloropɛrini nɔrɔlen na ni u ye BRN suguya vulkanizelen nɛrɛma fara a kan, u bɛ se ka vulkanizasiyɔn teliya, nɔrɔli tɛ dɔgɔya ni poliisosiyanati vulkanizecogo ye ani baga bɛ dɔgɔya kosɛbɛ.