Muonekano na Hali: Nyeupe (Uwazi au Translucent)
Aina ya tatu ya Monomer na Yaliyomo: ENB, 4.1%
Yaliyomo ya Ethylene: 53%
Mooney Mnato: ML (1+4) 125 ° C
saizi 30: 25kg/block
MOQ: Ufungashaji wa 25kg
: Boxed
Muonekano na Hali: Nyeupe (Uwazi au Translucent)
Aina ya tatu ya Monomer na Yaliyomo: ENB, 5.5%
Yaliyomo ya Ethylene: 68%
Mooney Mnato: ML (1+4) 125 ° C 87
saizi: 25kg/block
MOQ: 25kg
Ufungashaji: Boxed
Muonekano na Hali: Nyeupe (Uwazi au Translucent)
Aina ya tatu ya Monomer na Yaliyomo: ENB, 5.7%
Yaliyomo ya Ethylene: 71%
Mooney Mnato: ML (1+4) 125 ° C 24
size: 25kg/block
MOQ: Ufungashaji wa 25kg
: Boxed
Muonekano na Hali: Nyeupe (Uwazi au Translucent)
Aina ya tatu ya Monomer na Yaliyomo: ENB, 6.5%
Yaliyomo ya Ethylene: 68%
Mooney Mnato: ML (1+4) 125 ° C 135
saizi: 25kg/block
MOQ: 25kg
Ufungashaji: Boxed
Muonekano na Hali: Nyeupe (Uwazi au Translucent)
Aina ya tatu ya Monomer na Yaliyomo: ENB, 2.3%
Ethylene Yaliyomo: 57%
Mooney Mnato: ML (1+4) 125 ° C 35
saizi: 25kg/block
MOQ: 25kg
Muonekano na Hali: Nyeupe (Uwazi au Translucent)
Aina ya tatu ya Monomer na Yaliyomo: ENB, 9.4%
Yaliyomo ya Ethylene: 55%
Mooney Mnato: ML (1+4) 125 ° C 29
size: 25kg/block
MOQ: 25kg
Ufungashaji: Boxed