With years of experience in production LEV, Herchy can supply a wide range of LEV. LEV can meet many applications, if you need, please get our online timely service about LEV. In addition to the product list below, you can also customize your own unique LEV according to your specific needs.
Appearance and condition: Beige or pale yellow blocky Third monomer type and content: ENB, 5% Ethylene content: 70% Mooney viscosity: ML(1+4)100°C 30 Size: 25kg/block MOQ: 25kg Packing: boxed
Appearance and condition: Beige or pale yellow blocky Third monomer type and content: ENB, 4.5% Ethylene content: 55.5% Mooney viscosity: ML(1+4)125°C 76 Size: 25kg/block MOQ: 25kg Packing: boxed
Appearance and condition: Beige or pale yellow blocky Third monomer type and content: ENB, 5.5% Ethylene content: 69.5% Mooney viscosity: ML(1+4)125°C 80 Size: 25kg/block MOQ: 25kg Packing: boxed